I did search but with such a general term, didn't find the question exactly.
I use to use 50:50 Pb:COWW + added 95:5 solder to bring tin to 2%. WQ'ed.
Now, I have been using Rotometal Pb:No. 2 at 2:1, again WQ'ed.
I appreciate the Rotometal alloys. At the same time, I miss the ability to buy WW to make my own alloy. Not really a big deal to me to sort and smelt the dirty COWW.
It's been since about 2015. Are COWW's quickly becoming a thing of the past? For you guys who have traditionally used them, are you still sourcing them? If not, what are you subbing in for your alloy?