Nub questions for sure please excuse.
I've finally ran out of WW and I'm trying to figure out the best method to use going forward.
I've got 120 lbs of range lead that I have not melted yet and a small amount of pewter on hand. What would be the best route to get back to ingots around ~12 like I've been using? I guess my concern is how to get the variable of the range lead sorted out? Should I just make batches into ingots, then test the hardness, and then use the formula each time? I currently use a big iron skillet to melt but I know it's not going to hold that much. Maybe I should invest in a bigger pot? These are the questions that I hope others have already tackled.
Additional info, not new to casting but never used range lead, only used clip on and stick on wheel weights in the past. I plan to shoot mostly pistol non-magnum loads that are powder coated. Thought someone may could give me some direction to a good process for using range lead going forward.