Hey guys,
Been a minute since I’ve hit the reloading bench. Casting for my newly acquired 1895 and 1911 but hit a wall with powder coating.
HF red - 400F for 20 min and water cooled right after.
Worked before without issue, some look ok but some are flaking badly. Will melt those down and retry, curious if they didn’t have enough time to cure but 20min has worked in the past.