OK, I need some ?'s answered about doing this.
1) How critical is the temp? I know you can go too high and the lead will start to melt and the bullets will slump.
2) How low can you go on the temp and still heat treat them to a higher #?
3) What are you lubing the bullets with to size and check them before heat treating them?
4) How long do you let them sit after HT'ing them? I normally like to let my WD bullets sit for a couple of weeks if I can.
5) do you have to stand them up? Especially if you know you are going to use a lower temp.