Well, I have finally tried my new MP mold, https://www.mp-molds.com/product/359...ove-8-cav-alu/
very good mold, it is not difficult to produce many boolits in a short time
I have made them a layer of PC and left them for about 30 days before loading them, they weighed 175 grains, so their alloy is close to the Lyman No. 2
I loaded them with 13 grains of win 296, regular primers, and I have to say on my taurus 605 it was an angry mule
After 20 shots I didn't want to keep shooting.
I understand that win 296 is quite "special" with low loads, less than the minimum, are not recommended. But has anyone tried going below the minimum?
I would like to try 11 or 12 grains, to see if it is a more "hand-friendly" shot.
Needless to say, I didn't have good groups.