I have what is most likely a lifetime supply of lead, mostly smelted into reasonably clean ingots. Also have several hundred more pounds in a thick folded up sheet 3/16s thick. Problem is I had terrible luck casting pure lead and have he mostly successful with the 20to1 mix I you guys taught me about on this site. The problem i am having is while I have accumulated this much lead I have only found about 4 pounds of pewter. Can you guys help me find tin/pewter or something to make another alloy that will work as well as the 20to1 mix I like so much.