Elvis Ammo had this youtube " Powder Coat (As Much As We Can Lift) Where's The Limit?" that made PC look a lot easier and less fussy than I had previously seen.
https://www.youtube.com/watch?v=4LizyGKA4yQ
I have been using Lee "Mule Snot" lubing for my rifle boolets and found it messy and made my hands sticky. After seeing the cool colors of PC'd boolets I thought I'd like to try it.
I have a few questions though.
1, Can you use a #2 plastic tub, which is what my H-4198/H322 comes in? I thought #5 was the right stuff?
2. Elvis says he cooked at 275 degrees in this video, I thought that it had to be in the order of 400 degrees? He was using Eastwood blue powder. Is that different than what Smokes powder needs?
3. Anyone else tried this big batch process?
Some help here guys, before I invest in an oven and powder, please.