Does anyone use Babbitt Ingots as a source of tin for Bullet casting?
Roto Metals say theirs is 90-92% tin, 4-5% Antimony, 4-5% copper.
Mine one bar said Nickel XXXX, and the other 5# bar just says Hewitts Special Hardened Babbitt Metal. No other stamping or Number.