...starting with more reading to do. After about 3 years of sitting on this fence, I "get it". I have accumulated some of the basics:
cheap Thrift Store Toaster Oven (the heart of this effort)
1/4" grid galvanized hardware cloth (from another application), which isn't really 1/4" grid or was poorly Quality checked as it was spot welded
plastic tweezers for handling the boolits
4 to 5 thousand 223 boolits of 49-49-2 Pb-WW-Sn
and..."The Itch" to try PC
I will shortly obtain:
a Teflon mat to line the baking pan
some powder coating paint (Smoke's maybe)
a Cool Whip container for Shake and Bake
some Air Soft BB's from my boys
Question:
If the boolits, about 12-13 BHN, are baked for 20 minutes at (say) 425*F, will they not also be "heat treated" (to a degree) and harden over the coming days by this process?
From the Glen Fryxell and Robert Applegate book: