I have about 35 lbs of various range scrap lead (predominately jacketed stuff) that I've already made into ingots. The RS lead seems to soft for my full power 44 so I need to harden them up a bit. I can deeply gouge the boolits with my thumbnail when they are air cooled and make a bur that I can feel with my nail when water dropped.
I have approximately 17 lbs of lino that I can use to bring up the BHN but would like to know about how much lino will I need to add to get in the #2 alloy range. A bit softer then #2 will work as well as my normal alloy is a 50/50 mix of #2 and COWW. TIA