    Boolit recipes

    What is your best & cheapest recipe for turning my pure lead into cast boolit material .
    I see on line some material that is 65 1/2 lead - 23 antimony- 12 1/2 tin. I was thinking adding 15# of my lead to 5# of this. Would probably cost me about 40$

  2. #2
    Boolit Grand Master Tatume's Avatar
    Join Date
    Jan 2010
    Location
    VA
    Posts
    5,612
    Look in the Swappin & Sellin forum:

    http://castboolits.gunloads.com/foru...pin-amp-Sellin

    I looked, and the very first active thread was alloy for sale. You could mix 50/50 clip-on wheel weights, add tin (two pounds of 50/50 solder with 18 pounds of pure lead will make classic 20:1 alloy, or just add a big handful of linotype.

  3. #3
    Boolit Buddy

    cga's Avatar
    Join Date
    Jul 2009
    Location
    Bradford Pennsylvania
    Posts
    133
    If my math is correct...........
    2.5 lbs. of that alloy with 20 lbs. of your pure lead would be about the same hardness as clip on wheel weights, about 11.4 Brinell.

  4. #4
    Moderator Emeritus


    JonB_in_Glencoe's Avatar
    Join Date
    Mar 2010
    Location
    Land of 10,000 Lakes
    Posts
    15,957
    If I had a stash of pure (or near pure) Lead, and nothing else to blend with it, to make it a useful boolit alloy, I would search locally for Lino-type or Mono-type. Sometimes it can be found for near the price of scrap lead. Then I'd use the alloy calculator to formulate a blend for a desired application.
    ~~~~~~~~~~~~~~
    “If someone has a gun and is trying to kill you, it would be reasonable to shoot back with your own gun.”
    ― The Dalai Lama, Seattle Times, May 2001

  5. #5
    Banned
    Join Date
    Jul 2016
    Posts
    2,911

  6. #6
    Boolit Buddy
    Join Date
    Jul 2018
    Posts
    191
    Thank you, I went ahead & ordered that material. I have the lee .459 340 gr. Mold. Wii that 11.4 hardness work to push that boolit about 1800?

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check