ok, so in the lee 2nd edition book, 296 seems to produce less pressure on average then H110, on the other hand, in lyman cast boolit loading, H110 averages lower pressures. has anyone else noticed this? and which is correct? on the loads I saw it was usually a 12% difference ( I think that's right) for example one was 38,000 the other 34,000). if anyone knows this info needs to be shared because its pretty important. thank you very much, Travis