I use a homemade annealing machine, use 750 degree Tempilaq on a few cases and time them until they melt. Then i set my machine to that time average and go. I time cases again when I change brands. I record the times of case brands so I can repeat as necessary. I do not let my cases get glowing as neck tension is lost at that point.
That is what works for me. I am always open to suggestions of improvement.
YMMV
Slim