So I finally got around in ordering what I think is all the equipment I need to finally start casting my own boolits. I already have 2 Lee pots, 10 and 20# and of course the lead. Here's my question, I'm really only wanting boolits for plinking. I have 370+ pounds of CCWW, around 50 pounds of SOWW, and maybe 20 pounds of pewter tin. So many posts about mixes, and % its a bit confusing to me. I see most people use about 2% of tin to their CCWW lead, but what about the SOWW? Is this even necessary to mix in? I want to mix small batches at first, but what am I REALLY looking for when I cast? I'm very familiar with pouring lead for sinkers, but there is no need to worry about the imperfections I get with those. Obviously I know I want a nice, FULL boolit, but what else should I be looking for? These boolits will be shot from a Glock 19, and coated with the FAMED BB tumble in Harbor Freight powder. So leading shouldn't be any issues. I guess I just need to know if the SOWW is necessary to be mixed, if so how much to the tin and COWW and what exactly should I look for with the boolits after I pop them out? I'm sure it'll all make sense tomorrow when I get going, but wanted to ask now. Also, I've slugged my barrel at right around .355-.356 so I bought the .358 rezier kit. The molds I purchased both say they drop at .357, my assumption is after I coat them, they should be .359-.360 and the resizer should take care of that, correct? Lots of testing to do tomorrow, and I'm excited and nervous as I don't want anything to happen to my gun (or me) when I go to shoot them. Thanks everyone for the help!