Can anyone tell me the difference between these 2 chamber casting alloys? Is Cerrosafe worth the premium cost?
http://www.brownells.com/gunsmith-to...y-prod384.aspx
http://www.rotometals.com/product-p/...ting_alloy.htm
Can anyone tell me the difference between these 2 chamber casting alloys? Is Cerrosafe worth the premium cost?
http://www.brownells.com/gunsmith-to...y-prod384.aspx
http://www.rotometals.com/product-p/...ting_alloy.htm
Rotometals worked well for me. here:
http://castboolits.gunloads.com/showthread.php?209132-Test3-Hubel-FH-BlazingSabot-inspired-loads-and-pictures&p=2338792&viewfull=1#post2338792
and
http://castboolits.gunloads.com/showthread.php?209132-Test3-Hubel-FH-BlazingSabot-inspired-loads-and-pictures&p=2338794&viewfull=1#post2338794
C-
I had to order from Amazon since rotometals site kept giving me errors.
____________
"...the civil libertarians and rationalists who are ever on the alert to oppose tyranny "failed to take into account man's almost infinite appetite for distractions." In 1984, Orwell added, people are controlled by inflicting pain. In Brave New World, they are controlled by inflicting pleasure. In short, Orwell feared that what we fear will ruin us. Huxley feared that what we desire will ruin us. This book is about the possibility that Huxley, not Orwell, was right.” -N.Postman
I just got one from Rotometals.
Haven't tried it yet.
Looks strange. But I have nothing to compare it to, so I'll just try it and see what happens.
I the old days we used sulphur and I had a chart for shrinkage after so many hours. I bought my Cerro safe years ago and it's still working so if you figure in 20 years of use it's not so bad.
KSCO I have had sulphur or sulfur chamber casts made decades ago but someone else did them. Can you tell me where to get directions on doing one and where to get materials? Thanks! Chill Wills
Chill Wills
I'm willing to bet the Rotometals alloy is the same as cerrosafe. You need the time / shrinkage chart for those.
Sulpher mixed with powdered graphite does not shrink or expand once cooled and makes measurements a little more straight forward. It does require a higher melting temp though.
I bought the cerrosafe before I knew that Rotometals had an alternative.....subsequently, a buddy bought rotometals....I have used some of his (their smallest qty is pretty much a lifetime supply!) and I think they are the same. Rotometals is a deal if you have a buddy to share with. Both Brownells and Rotometals are four star outfits to deal with.
BP | Bronze Point | IMR | Improved Military Rifle | PTD | Pointed |
BR | Bench Rest | M | Magnum | RN | Round Nose |
BT | Boat Tail | PL | Power-Lokt | SP | Soft Point |
C | Compressed Charge | PR | Primer | SPCL | Soft Point "Core-Lokt" |
HP | Hollow Point | PSPCL | Pointed Soft Point "Core Lokt" | C.O.L. | Cartridge Overall Length |
PSP | Pointed Soft Point | Spz | Spitzer Point | SBT | Spitzer Boat Tail |
LRN | Lead Round Nose | LWC | Lead Wad Cutter | LSWC | Lead Semi Wad Cutter |
GC | Gas Check |