I am on the hunt for or going to make some ingot moulds.
Looking for 6-8 lb ingots from ww's.
I know lead won't stick in cast iron, aluminium or stainless.
I want to do this once, so quality is a primary concern. I want to make enough to pour 80-90 ingots at one time.
Suggestions for dimensions, materials and design needed. The ingots will then feed a Lee 4-20 pot.
Cheap would of course be good, availability will factor in to a lesser degree, something I could find/fabricate from local resources would be great.
If I can find/make something that turns out ingots that are reasonably easy to stack would be great.
I'm currently using muffin tins made out of aluminium, but the weight of the muffins when full (12 muffin tin) is taking it's toll on them. I don't expect them to last much longer.
Thanks in advance for the help