I’ll wash my brass using pins and a tumbler. I’ll then set them on a sunny place to dry. The summer Texas sun will anneal them while they dry. Lol
I’ll wash my brass using pins and a tumbler. I’ll then set them on a sunny place to dry. The summer Texas sun will anneal them while they dry. Lol
The sooner I fall behind...the more time I have to catch up with
I just built my own annealer. I use tempilaq on the inside of the case mouth and when it liquifies and turns translucent, then I know it is done.
I use this to see if it will extend the life of my brass. It doesn't take too long with a somewhat automated machine. About 6 seconds for a 30-06 case, so 10 a minute. That's faster than all of my other steps.
This is by far the biggest bang for the buck I have found for annealing cases. It works wonderfully.
https://www.youtube.com/watch?v=jLRgDZeYQ-M
NRA Benefactor +, GOA Life, GONH Life, CRPA Life, SAF Life
BP | Bronze Point | IMR | Improved Military Rifle | PTD | Pointed |
BR | Bench Rest | M | Magnum | RN | Round Nose |
BT | Boat Tail | PL | Power-Lokt | SP | Soft Point |
C | Compressed Charge | PR | Primer | SPCL | Soft Point "Core-Lokt" |
HP | Hollow Point | PSPCL | Pointed Soft Point "Core Lokt" | C.O.L. | Cartridge Overall Length |
PSP | Pointed Soft Point | Spz | Spitzer Point | SBT | Spitzer Boat Tail |
LRN | Lead Round Nose | LWC | Lead Wad Cutter | LSWC | Lead Semi Wad Cutter |
GC | Gas Check |