I have 6 @ FRSBs of pure lead, that I’d like to TRADE for harder alloys.
Source was reclaimed lead pipe, from broken water mains. No solder, or other joints included.
Melt was fluxed several times, with saw dust, then wax.
Was double checked, with Muriatic Acid- No Reactions.
Lee BHN Tester yielded consistent 4.5 - 5 BHN on random samples.
Muffin tin yielded approximately, 2-1/4 x 3-1/2 x 1-5/8 ( Hand Soap Bar Size ) @ approximately 3.3 - 3.5 lbs.
Lee mold 1’s
Each cover shipping.
Box 1 20.34 lbs. Hondolane’s. SHIPPED
Box 2 20.21 lbs. Hiwall55’s. SHIPPED
Box 3 19.84 lbs. Jevyod’s. Shipped
Box 4 19.84 lbs. Green Frog’s. SHIPPED
Box 5 19.84 lbs. SSGOldfart’s. SHIPPED
Box 6 19.46 lbs. hawkenhunter50’s. SHIPPED
Please DM/PM ,
Kenny