Load DataWidenersLee PrecisionRotoMetals2
Titan ReloadingInline FabricationReloading EverythingRepackbox
MidSouth Shooters Supply
Results 1 to 7 of 7

Thread: Purify lead

  1. #1
    Boolit Buddy JLF's Avatar
    Join Date
    Apr 2021
    Location
    Alvarez (ARGENTINA)
    Posts
    158

    Purify lead

    When melting the lead to form the ingots, the lead has impurities. Is any substance added to properly separate these impurities?
    "When the homeland is in danger, everything is allowed, except not to defend it."

    Gral. Don José de San Martin.

  2. #2
    Moderator


    Winger Ed.'s Avatar
    Join Date
    May 2007
    Location
    Just outside Gun Barrel City, Texas
    Posts
    9,484
    Get it a little hotter than the melting temp. then flux, scrape the bottom & sides and stir like it owes you money.
    All the trash & such will float to the top so you can skim it off.

    I've done that with the dirtiest Lead from buried cable sheathing,
    and even the nastiest Lead from old school cast Iron sewer pipe joints.

    After 2-3 go arounds, it'd didn't even smell like crap any more.
    Last edited by Winger Ed.; 12-11-2022 at 12:22 PM.
    In school: We learn lessons, and are given tests.
    In life: We are given tests, and learn lessons.


    OK People. Enough of this idle chit-chat.
    This ain't your Grandma's sewing circle.
    EVERYONE!
    Back to your oars. The Captain wants to waterski.

  3. #3
    Boolit Master
    Join Date
    Apr 2016
    Location
    NC
    Posts
    2,863
    It depends upon what the impurities are.
    Dirt, ash, and other things that are not metal are easily removed by fluxing and skimming as described above.
    If the impurity is another metal, for example tin, zinc, or copper that is a part of the melted lead alloy, there is no way to readily and safely remove it in a home environment.

  4. #4
    Boolit Buddy JLF's Avatar
    Join Date
    Apr 2021
    Location
    Alvarez (ARGENTINA)
    Posts
    158
    What do you use as a flux? Could it be candles?
    "When the homeland is in danger, everything is allowed, except not to defend it."

    Gral. Don José de San Martin.

  5. #5
    Boolit Buddy 414gates's Avatar
    Join Date
    Jan 2017
    Posts
    357
    Quote Originally Posted by JLF View Post
    What do you use as a flux? Could it be candles?
    I use ash, and I stir with a charred wooden stick.

    The dirtiest I've had was a blob of lead that was spilt on the floor in a foundry, it had bits of sand, etc, which just floats off the melt anyway.

    I bought some sulphur once, in case of zinc contamination, but so far I've only used it for a chamber cast.

  6. #6
    Boolit Master deces's Avatar
    Join Date
    Nov 2012
    Location
    noyb
    Posts
    758
    These men and their hypnotized followers call this a new order. It is not new. It is not order.

  7. #7
    Boolit Buddy JLF's Avatar
    Join Date
    Apr 2021
    Location
    Alvarez (ARGENTINA)
    Posts
    158
    Thank you very much for your help.
    "When the homeland is in danger, everything is allowed, except not to defend it."

    Gral. Don José de San Martin.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check