Since I'm doing big batches of coating while casting boolits I would like to heat treat some of the boolits the next day or two. I sometimes get in a hurry before leaving for my afternoon shift, and things does not always go as planned. I'm sure you know.
Has anyone tried this after applying the coating with acceton? The longest I've waited until now is a couple of hours before getting them into the oven.
If drying in a dust free environment impact the coating and its properties in any negative way I'll not do this. This is in my heated casting shop. So it newer gets cold or humid in any way.
Thanks
Sent fra min YAL-L21 via Tapatalk