Thread: Got serious about melting lead

  1. #21
    Boolit Master
    Join Date
    May 2008
    Location
    Plymouth County, IA
    Posts
    708
    That fella in the video must not have known you can dump the ingot molds in about a miniute and reused them...like a bullet mold...if you want a 1,000 boolits, you don't need 1,000 cavities! A nice little unit.
    Take a kid to the range, you'll both be glad you did.

  2. #22
    Boolit Master

    fivegunner's Avatar
    Join Date
    Aug 2005
    Location
    LOWELL Michigan
    Posts
    713
    Nice pot!

  3. #23
    Boolit Buddy
    bluebird66's Avatar
    Join Date
    Dec 2018
    Location
    SW VA
    Posts
    114
    Great setup!

  4. #24
    Boolit Master

    Join Date
    Oct 2013
    Location
    JAX, FL
    Posts
    1,230
    Quote Originally Posted by Buck Shot View Post
    that feller right there has a near fortune tied up just in ingot molds. But it gives us an indication of volume/capacity, 16 molds X 4 pounds = 64 pounds in 5 minutes. Pretty nice.

    I'd surely like to see what type valve or mechanism is used.

    Correction: the video was/is the builder of the pots and he explains his demonstration in a reply to a question in the comments. He used the Lee 1 and 1/2 pound combination ingot molds. So he poured 45 pounds.
    Last edited by oley55; 08-31-2021 at 02:05 PM.
    “Some people spend an entire lifetime wondering if they made a difference in the world. But, the Marines don't have that problem.” Ronald Reagan


Page 2 of 2 FirstFirst 12

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check