Titan ReloadingMidSouth Shooters SupplyWidenersRepackbox
Load DataLee PrecisionReloading EverythingInline Fabrication
Snyders Jerky RotoMetals2
Results 1 to 13 of 13

Thread: Melted some ww today...

  1. #1
    Boolit Man
    Join Date
    Mar 2008
    Location
    Sweden
    Posts
    89

    Melted some ww today...

    and i was a little depressed with how much iron and ZN weights there was in there Well i got some 47kg out of 1 and a 0.5 25L buckets and i only had 500sek (about 55$) in it so it wasn´t all that bad i think. What do you all think ? And i learned that it is probably not a good idea leaving the buckets alongside my fathers garage too collekt rain whilst you go abroad for a tour in Afghanistan, man were they rusted

    Happy shooting all
    Math

  2. #2
    Boolit Master Cowboy_Dan's Avatar
    Join Date
    Jun 2014
    Location
    Northern Indiana
    Posts
    701
    A little over US$1 per kg is pretty good in my book. My last batch came to just under $1 per pound (.454 kg) when I removed the zinc and steel.
    "It is wrong always, everywhere, and for everyone to believe anything on insufficient evidence."
    -W. K. Clifford "The Ethics of Belief"

    "They hate you if you're clever, and they despise a fool."
    -John Lennon "A Working Class Hero"

  3. #3
    Boolit Master
    Join Date
    Mar 2014
    Location
    St. Louis
    Posts
    2,046
    That's right at 66% and I've gotten buckets that were far worse.

  4. #4
    Boolit Bub
    Join Date
    Apr 2014
    Posts
    56
    I think I got about 30% in the Atlanta area. Unless I knew what yield I could expect, I would't be willing to pay more than about $0.25 / pound for unsorted wheel weights.

    Main problem I have is getting hard lead. Only about 25% of the lead I got was clip on. 75% was stick on. The bright side is it forced me to expirment with very soft alloys. I have learned that most of the time [with pistols] you don't need that hard of an alloy.

    Good job with that find. The thrill of finding cheap lead, tempered only with the chore of sorting.

    -Ben

  5. #5
    Boolit Man
    Join Date
    Mar 2008
    Location
    Sweden
    Posts
    89
    Ok from what i hear i did reasonable good then. I must say i had some problem getting the heat up and keeping it up. I think i need too adjust my smelting teknik, ideas are most welcomed ! My setup today was a stainless pot a 1500L propan burner that i could not get straight under the pot,could be that i lost a fair amount of heat by using a angeled burner ?
    Math

  6. #6
    Boolit Bub
    Join Date
    Apr 2014
    Posts
    56
    Are there any flames along the side of the pot? If so, that's wasted heat. If the burner is angled, but is still centered under the pot it should still be fine.

    Try putting lots of sawdust on top of the melt. It'll flux and insulate the alloy like a blanket. Also try making a foil heat shield around the burner to allow air in but keeps the heat from radiating out (look at small back-packing camp stoves. They have heat shields).

    -Ben

  7. #7
    Boolit Grand Master

    Join Date
    Oct 2009
    Location
    England,Ar
    Posts
    7,700
    Glad you are back from Afghanistan and able to melt lead! I'm not sure what differences one would see between Sweden and the US with whats available, but lots of guys here use a Turkey fryer and a cut off propane tank, or a large dutch oven. Google Cajun cooker or Bayou classic to see a few examples. A few like me even use a homemade burner and stand. I can melt 400# in about 20 minutes, but it drains the propane tank really quick. Also, look at a few of the stickies for a few ideas and see what other members are using!

    The yield from wheel weights varies from place to place. My last batch was very good, but others are reporting yields low enough that they are leaving wheel weights for other sources. Good Luck in your search for lead.

  8. #8
    Boolit Man
    Join Date
    Mar 2008
    Location
    Sweden
    Posts
    89
    Thanks for the kind remarks I`m sorry to say were not big on frying turkeys here i Sweden so finding a cheep fryer is a longshot. Just saw that my stainless pot had come apart at the bottom, so i think i need to find me a sturdier vessel for melting in and a improved wind shelter. Any thoughts on what material that vould be best, stainless or ordinary steel ?
    Math

  9. #9
    Boolit Buddy
    Join Date
    Dec 2005
    Location
    Oroville CA
    Posts
    235
    A thicker standard steel works very good as It helps conduct and retain heat. Cold rolled steel pipe with the end sealed with a welded plate is what I use. For A heat source and stand I bought a 150,000 BTU bronze burner and mounted it inside a sand rail rim that I modified. The only cost for the whole set up was the burner. The rest was sourced from scrap piles. Allows me to process about 350 lbs of finished melt in an hour.
    The very young do not always do as they are told.

  10. #10
    Boolit Master
    Join Date
    Mar 2005
    Location
    B.C. Canada
    Posts
    2,725
    A pot can be made from an old 20 pound propane cylinder. Screw out the valve, fill the tank with water, use a zip-cut tool to cut a larger hole in the top of the tank. Next, dump out the water, lay the tank on its side and cut around the circumference close to the "shoulder" on the tank. A makeshift burner can be made using a Tiger torch, a 45 degree steel, galvanized or cast pluming elbow and 4 cement building blocks. Place the elbow on the ground, held in place by the 4 blocks. Set the tank over the hole in the middle of the blocks and place the tiger torch in the lower end of the elbow. Fill (or whatever) the pot with scrap, light the torch and away you go. Be prepared to dip the melted metal out of the tank---you for sure will not lift it to pour! Have fun!
    R.D.M.

  11. #11
    Boolit Bub
    Join Date
    Apr 2014
    Posts
    56
    If you have access, I'd lean toward stainless. Much easier to keep to clean.

  12. #12
    Boolit Man
    Join Date
    Mar 2008
    Location
    Sweden
    Posts
    89
    Thanks for all input I guess it comes down too what sort of material i find first then I`m sort of contenplating making a square one out of 5mm checker plate, square so it will fit my currant stand But thats a little more job so i guess i go looking for some suitable pipe to hack a pice of
    Math

  13. #13
    In Remembrance


    Join Date
    Oct 2008
    Location
    Michigan Thumb Area
    Posts
    5,948
    A friend of mine bought a 10" long piece of 10" diameter weldable pipe from a scrap yard. He then had a 5/16" thick steel bottom welded on of plate steel by a professional welder. He has been smelting lead weights in this homemade pot for the last 12 years on a heavy duty homemade tripod and using several high output propane torches for heat.Robert

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check