One thing I have trying to do for warm boolits is after pulling baked boolits out of the oven is to put a second coat on after they have cooled to about 25-30 deg C.(Just warm to the touch) At 1deg C ambient it doesn't take very long.
Last bunch I used 5-1-8 mix on the HT_TEK Black and 120ml-20g on Red Copper powder.
Question, Can I over coat at these mixes?
There is no liquid mix in the bucket when I dump them on the drying screen after about 15 to 20 sec of tumbling .