    Lightbulb more coatings

    I've found two more items that looked promising a lube; an aerosol wax intended as a mould release agent for use with vacuum forming plastics and the other a water based acrylic liquid intended as a sealer for MDF and wood surfaces.

    Test vehicle was my Mosin 1891. Load was my standard accuracy load of the Lee .311-185 bullet and 28gr. of Lovex D060 (aka Accurate 5744) which gives consistent grouping at 2100 fps. I know this is a tough test to start out with but these were the only bullets I had cast up, gas check seated, but not lubed. Ten rounds of each were loaded and shot at 50 metres, prone but with no sling or other support.

    Here is the spray wax. The supplyer is in the uk but this was not made by them so I suggest you just look for a product with the same description for the same intended application.
    Click image for larger version. 

Name:	wax-label.JPG 
Views:	28 
Size:	37.1 KB 
ID:	64809Click image for larger version. 

Name:	wax-rear label.JPG 
Views:	25 
Size:	50.6 KB 
ID:	64810

    I gave two applications of the spray and when dry the bullets felt quite slippery and slightly tacky, like on some brands (RWS, Remington) of .22 rimfire ammo.

    Click image for larger version. 

Name:	mosin_wax.jpg 
Views:	43 
Size:	23.6 KB 
ID:	64812

    Grouping was good, all the holes were round and there was no sign of lead fouling in the barrel. So this one is worthy of more testing.

    The MDF sealer is by Rustins which is a multi national so it should be available at your local DIY wood working supply store. Application was by simply dipping the bullets and leaving to dry for half an hour. Once again two coats were applied.I notice they also do a product called "liquid wax" that looks worth a try.

    Click image for larger version. 

Name:	mosin_mdfsealer.jpg 
Views:	25 
Size:	20.3 KB 
ID:	64813

    Grouping is not as good as I was getting tired, note the called flyers. This time there were ovular holes and clearly visible lead fowling. I will not be using this again.
    "Consciousness is a lie your brain tells you to make you think you know what you are doing." Professor Maria Goncalves.

    If liberty means anything at all, it means the right to tell people what they do not want to hear. George Orwell.

  2. #2
    Boolit Grand Master popper's Avatar
    Join Date
    Jun 2011
    Posts
    10,586
    Looks interesting, pretty good at that fps.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check