Snyders JerkyTitan ReloadingWidenersLoad Data
RepackboxLee PrecisionMidSouth Shooters SupplyReloading Everything
RotoMetals2 Inline Fabrication
Page 16 of 17 FirstFirst ... 67891011121314151617 LastLast
Results 301 to 320 of 321

Thread: MiHec 360640 Light brass four cavity HP or four cavity solid

  1. #301
    Boolit Buddy Low Budget Shooter's Avatar
    Join Date
    Feb 2010
    Location
    Texahoma
    Posts
    464
    Woohoo! The wait has been so long, I can hardly believe it's finally done. I don't think I've ever turned over $100 so happily in my life.
    I'm not sure where all the money is that I've "saved" by casting and reloading!

  2. #302
    Boolit Grand Master

    dragon813gt's Avatar
    Join Date
    Feb 2012
    Location
    Somewhere in SE PA
    Posts
    9,989
    829 days from being the first to sign up to sending payment

  3. #303
    Boolit Grand Master
    rintinglen's Avatar
    Join Date
    Jul 2007
    Location
    Orange, VA NOW
    Posts
    6,524
    Holy moly! it's here at last. On the plus side, the decline of the euro in value means that this one will cost me a smidgen less than than last, if the Paypal Currency converter is to be trusted.
    _________________________________________________It's not that I can't spell: it is that I can't type.

  4. #304
    Boolit Buddy AZBrian's Avatar
    Join Date
    Sep 2013
    Location
    Chandler, AZ
    Posts
    108
    Received Invoices for both moulds and made Payment for each.

    A long wait for this one - will be very happy to get them!

    Thanks!!
    AZBrian

  5. #305
    Boolit Master
    GLL's Avatar
    Join Date
    Mar 2005
    Location
    California
    Posts
    3,580
    Now the wait for the 361627 !

    Jerry
    S&W .38/44 Outdoorsman Accumulator

  6. #306
    Boolit Man

    Join Date
    Mar 2014
    Location
    Southeast AZ
    Posts
    96
    Awesome, paid.

  7. #307
    Boolit Master wonderwolf's Avatar
    Join Date
    Apr 2007
    Posts
    1,655
    Excellent! Paid! Thanks again....what mold is next on your list MiHec?
    My firearms project blog

  8. #308
    Boolit Master Stick_man's Avatar
    Join Date
    Mar 2009
    Location
    Salt Lake City, UT
    Posts
    543
    Invoice has been paid! Looks like Christmas in April or May this year. Can hardly wait.
    "We the people are the rightful masters of both
    Congress & the courts, not to overthrow the Constitution,
    but overthrow the men who pervert the Constitution."

    Abraham Lincoln

  9. #309
    Boolit Buddy
    rockydoc's Avatar
    Join Date
    Aug 2013
    Location
    Northwest Florida
    Posts
    104
    Quote Originally Posted by rockydoc View Post
    I would like a 4 cavity Cramer with plain base and large hp and solid pins.
    harley dot rock at knology dot net
    I placed my order 11-4-14 and received notice the order was ready and sent my payment 4-17-15. Approximately 6 ½ months, that's not too bad. How long does it take for an order to arrive from Europe?
    NRA Lifetime member since 1956, NRA Endowment Member. Reloading since 1954. CBA Member Navy Vietnam Veteran USS Intrepid CVA 11

  10. #310
    Vendor Sponsor

    MiHec's Avatar
    Join Date
    May 2008
    Location
    Europe
    Posts
    2,500
    Quote Originally Posted by rockydoc View Post
    I placed my order 11-4-14 and received notice the order was ready and sent my payment 4-17-15. Approximately 6 ½ months, that's not too bad. How long does it take for an order to arrive from Europe?
    In normal conditions - around 14 days
    www.mp-molds.com
    --------------------------------------
    If you want to win, you must not lose

  11. #311
    Boolit Buddy
    LabGuy's Avatar
    Join Date
    Sep 2010
    Location
    Tallahassee Florida
    Posts
    348

    It's here

    I just got mine!


    Click image for larger version. 

Name:	IMG_0142.JPG 
Views:	39 
Size:	99.1 KB 
ID:	138113

  12. #312
    Boolit Buddy Low Budget Shooter's Avatar
    Join Date
    Feb 2010
    Location
    Texahoma
    Posts
    464
    Got mine today, too. Thanks 45 2.1 and Miha! LBS
    I'm not sure where all the money is that I've "saved" by casting and reloading!

  13. #313
    Boolit Buddy
    rockydoc's Avatar
    Join Date
    Aug 2013
    Location
    Northwest Florida
    Posts
    104
    Quote Originally Posted by rockydoc View Post
    I placed my order 11-4-14 and received notice the order was ready and sent my payment 4-17-15. Approximately 6 ½ months, that's not too bad. How long does it take for an order to arrive from Europe?
    I received the mold today, 10 days after payment. Not bad. I am pleased with everything: what I got and the amount of time it took, except it came with no instructions. This is my first brass mold, so are there any special preparations to do to get it ready to cast other than lubricating the alignment pins and sprue plate hinge?
    NRA Lifetime member since 1956, NRA Endowment Member. Reloading since 1954. CBA Member Navy Vietnam Veteran USS Intrepid CVA 11

  14. #314
    Boolit Master Stick_man's Avatar
    Join Date
    Mar 2009
    Location
    Salt Lake City, UT
    Posts
    543
    Got mine today. Can't wait to try it out, although it will likely be a little while.

    Rockydoc, I scrub my mold and pins down real good with brake cleaner, then hot soapy water, then brake cleaner, then one more time with the hot soapy water. Rinse it off well and let it dry. Then install the pins that I want to use and lube the key points. Then I do a couple cycles of heat and cool. One more touch of lube and I am ready to start casting. I preheat my molds on a hotplate. Usually getting nice pretty boolits within just a few drops.
    "We the people are the rightful masters of both
    Congress & the courts, not to overthrow the Constitution,
    but overthrow the men who pervert the Constitution."

    Abraham Lincoln

  15. #315
    Boolit Master
    Join Date
    Jun 2008
    Location
    TWIN CITIES
    Posts
    727
    Received mine today as well. Looks perfect as always! Thanks again for a great mould.

    ward
    "To anger a conservative, lie to him. To anger a liberal, tell him the truth." —Theodore Roosevelt"

  16. #316
    Boolit Bub
    Join Date
    Nov 2014
    Posts
    38


    360-640 and his little brother 360-640L

    20:1 about 146gn and 126gn respectively with the deep cavity pins. Now another excuse to buy more lead.
    Last edited by Jlamont2020; 04-28-2015 at 02:16 AM.

  17. #317
    Boolit Master
    Join Date
    May 2012
    Location
    Alaska
    Posts
    1,601
    I was pleasently surprised to find a package on the kitchen table containing another beautiful MP mold last night!

  18. #318
    Boolit Master
    Join Date
    May 2012
    Location
    Alaska
    Posts
    1,601
    Quote Originally Posted by rockydoc View Post
    I received the mold today, 10 days after payment. Not bad. I am pleased with everything: what I got and the amount of time it took, except it came with no instructions. This is my first brass mold, so are there any special preparations to do to get it ready to cast other than lubricating the alignment pins and sprue plate hinge?
    The only difference I find with brass compared to steel and aluminum is it seems to be a bit more finicky with temperature, i.e. not to hot, not to cold but just right. Just give it a nice pre-heat and as with any other mold give it some time for you to find the right temp and cadence. If it's your first hp mold, beware that you need to cast fairly quickly to keep the heat in the pins so that you get a complete fill out.

  19. #319
    Vendor Sponsor

    MiHec's Avatar
    Join Date
    May 2008
    Location
    Europe
    Posts
    2,500
    I have some overorder molds. If you want one send me PM
    www.mp-molds.com
    --------------------------------------
    If you want to win, you must not lose

  20. #320
    Boolit Grand Master
    rintinglen's Avatar
    Join Date
    Jul 2007
    Location
    Orange, VA NOW
    Posts
    6,524
    It got all the way from Slovenia to Huntington Beach where some feckless illiterate postal employee managed to mislay, or mis-deliver it. This positively stinks.
    _________________________________________________It's not that I can't spell: it is that I can't type.

Page 16 of 17 FirstFirst ... 67891011121314151617 LastLast

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check