  1. Replies
    6
    Views
    1,556

    It's probably Ammoload brass. I cull these and...

    It's probably Ammoload brass. I cull these and discard them because the internal case volume is reduced by the constriction.
  2. Neither acetone nor mineral spirits removed the...

    Neither acetone nor mineral spirits removed the Hi-Tek coating. Into the production pot they go.
  3. it was a mixture of HF red and some white I...

    it was a mixture of HF red and some white I scrounged from a powder coating shop. This combination has worked fine on bare boolits. I might try again with some Super Wet Black.
  4. OK, I just started soaking two test samples of...

    OK, I just started soaking two test samples of Hi-Tek coated boolits -- one in acetone and one in mineral spirits. Tomorrow I'll see whether either dissolved the coating.
  5. I just tried tumble coating the H-Tec coated...

    I just tried tumble coating the H-Tec coated boolits and the powder wouldn't stick.
  6. Banger, I'm not sure soaking in a solvent would...

    Banger,
    I'm not sure soaking in a solvent would help. One of the tests used to determine if the Hi-Tek coating is properly done is whether the coated boolits pass the "acetone test". This involves...
  7. Powder coating previously Hi-Tek coated boolits

    Before I switched to dry tumble powder coated I used the Hi-Tek coating method and I still have a bunch of Hi-Tek coated boolits on hand. Has anyone recoated Hi-Tek coated boolits with powder coat...
  8. Replies
    7
    Views
    1,936

    Powder poops out - powder fatigue?

    I powder coated a bunch of Lee 358-105-SWCs and 356-102-1Rs with HF red using the Cool Whip airsoft BB shake and bake method. I shook batches of about 30 at a time and used forceps to transfer them...
  9. Replies
    19
    Views
    3,283

    My alloy is 92% lead, 6% antimony and 2% tin and...

    My alloy is 92% lead, 6% antimony and 2% tin and the Brinell Hardness Number is 18. I buy ingots from Texas Lead Company in Houston. Thanks for the grit paper suggestion -- I'll try it.
  10. Replies
    19
    Views
    3,283

    Yes, I use a Lyman M die.

    Yes, I use a Lyman M die.
  11. Replies
    19
    Views
    3,283

    There weren't any fins on the cast boolits before...

    There weren't any fins on the cast boolits before sizing, only after sizing.
  12. Replies
    19
    Views
    3,283

    Lee's web site shows that the punch for their...

    Lee's web site shows that the punch for their .358 sizing die has a diameter of .353. Where did you get two other sizes, and what are their diameters? The boolits I have a problem with are from the...
  13. Replies
    19
    Views
    3,283

    I did that and it does keep the bases flat. ...

    I did that and it does keep the bases flat. However, the boolits end up looking a lot like wadcutters. I'll try shooting them this way anyway. It sure beats remelting and recasting.
  14. Replies
    19
    Views
    3,283

    Lee sizer punches too small

    Lee's sizer punches for their .356, .357, and .358 resizing dies all have a diameter of .353. I find that if I have an oversize 38 special boolit the punch diameter is too narrow and the boolit gets...
  15. Humidity is bad - it keeps the powder from...

    Humidity is bad - it keeps the powder from sticking.
  16. Replies
    24
    Views
    9,916

    What kind of gloves do you use?

    What kind of gloves do you use?
  17. Sticky: Yes - powderbuythepound.com. You can also order...

    Yes - powderbuythepound.com. You can also order from allpowderpaints.com. They have cheaper prices and cheaper shipping. Super Durable Wet Black works great.
  18. Powder coating lead balls for percussion revolvers

    Has anyone tried coating soft lead balls used in percussion cap and ball revolvers? I just ordered a Pietta 1858 Remington New Army replica revolver. I wonder whether there would be any benefit to...
  19. Replies
    291
    Views
    152,129

    I agree. I get much better results using...

    I agree. I get much better results using aluminum screen than I did with stainless hardware cloth. Boolits would stick fast to the hardware cloth and removing them would pull paint off, exposing...
  20. Replies
    2
    Views
    1,554

    Acetone test for powder coated boolits?

    I tried Hi-Tek coating before moving to shake and bake powder coating. With Hi-Tek coating there are two tests for determining whether the process was done correctly -- the smash test and the...
  21. Replies
    314
    Views
    391,091

    Sticky: Please pardon this newby question, but how much...

    Please pardon this newby question, but how much is a "light crimp"? I have stopped using my Lee factory crimp dies (because they tend to swage down the boolit diameter) and just use the seating die...
  22. Replies
    14,837
    Views
    5,187,305

    Sticky: I'd like to know how to determine coating volumes...

    I'd like to know how to determine coating volumes for different size boolits. Is there a linear relationship between boolit weight and surface area? If so, a 200 grain boolit would need twice as...
  23. Replies
    14,837
    Views
    5,187,305

    Sticky: Is that with one or two coats?

    Is that with one or two coats?
  24. Replies
    14,837
    Views
    5,187,305

    Sticky: I used a Harbor Freight digital micrometer. The...

    I used a Harbor Freight digital micrometer. The TL452-230-2Rs I cast measured 453. I made both batches in the same casting session.
  25. Replies
    14,837
    Views
    5,187,305

    Sticky: I coated my first boolits the other day with...

    I coated my first boolits the other day with Donnie's dark green. I double coated some Lee TL452-230-2Rs into 45ACP and 45 Colt cases and shot them through my Ruger Blackhawk convertible -- no...
Results 1 to 25 of 37
Page 1 of 2 1 2
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check