Powder coating in the south
I'm sure this has been answered before, and if so, just point me to the previous post.
If not, here we go.
Does the dry tumble/shake n bake method work in the south? Is it hard to get a static charge built up with high temps and high humidity like we have in the summer?
Im using Hiteks wet method right now, and I like it, but we are all experimenters, so I want to try something new.
Sent from my SM-G955U using Tapatalk
Powder coating in the south
Dude...the South got air conditioning in, like, 1954... [emoji1783] No problems doing it in the A/C.