Ok so today got off early from work and decided to make some caps. Made the H42 with .02 gr aluminum added this is a 100 gr recipe, packed the caps. Used a rod that has a small pistol primer cup soldered to it for a measure. Then i took the same small pistol measure and put 6 cups of bulseye in a shot glass with a table spoon of acetone and let it sit for ten minutes then stirred till dissolved then added a drop to each cup then let it sit for 10 minutes the hit with blow dryer on high heat for a minute or so then into the toaster oven on around 170 F for 15 minutes. Once it was cool i sprayed it with a thin coat of lacquer to hopefully make it more resistant to humidity. Let it dry then tested some of them with a hamer on a steel plate. I think that bullsey deluted in acitone makes a difference, alot louder and hed a pice of cap materiel shoot through my sweat pants and into my leg. Nothing serious but stung a bit. Wasn't expecting that. I think these are going to be a bit hotter than the regular one i have been making. Please let me know if im heading up the wrong path here with this. All i want is good home made caps that are reliable. I will explain that next poast.