Originally Posted by
Frankv
I have never used Hi-Tek.
Originally I tried HF PC, worked, but difficult to work with.
This silicone powder is simple ,cost effective and the finished product looks an works great. I am currently casting and coating 1k of 125 9mm.
My original 380's I did 150 and I was so impressed that I did 1000 and they all exceeded my expectations.
The most impressive part is the HF PC finished coated .360 102gr had to be lubed to be sized,the silicone coated at .360 finish coat effortlessly sized at .356 with no lube.These have a slick feel to them,but a hard finish.they don't stick to the alloy pan that i bake them on.This is cheap,fast and efficient.