Originally Posted by
Dusty Bannister
I do know, that's why I called LEE to ask what their alloy is.
Their reply is they don't have an alloy, they are not allowed to have lead on the premises.
So they have never used their own Molds
Utter B S, I will type part of the instructions that came with their two cavity molds.
"All bullet weights for Lee bullets are given using a one-to-ten lead/tin mix, except round balls and minis. These are designed to use pure lead."
Technically, they do not use an alloy, they use a mix.