I'll trade you one for one clean WW lead for one clean pure lead. It'll solve your problem with getting harder lead and solve my problem of not having enough soft lead.
Edd
Printable View
Pure lead and lino mixed 50/50 is what Rotometals call Magnum Metal. It is good stuff. About 2% Sn, 6% Sb, the rest Pb, and about as strong as one could realistically need for casting boolits. Actually, TOO hard for most of our efforts, but still Good Stuff!