excess650
06-17-2010, 08:10 PM
Does anyone have a reference that lists the composition of Westinghouse #25 alloy?

MtGun44
06-17-2010, 09:22 PM
I'm betting it is a tin lead babbit, which typically has some copper to strengthen it, but no
references.

Bill

excess650
06-17-2010, 11:29 PM
I'm inclined to think it one of the 50%+ lead babbitts as the bars weigh about 5.5# and are harder than lino.