Johnch
03-22-2023, 11:19 AM
Not sure if this is the right place
So if not feel free to move it
OK I make some of my own shot
Drip and roll into a cooling tank method
But I got to thinking last night
We do a lot of Morning Dove hunting as we wait for the Canada geese to decide to fly
As we are going to be also hunting geese , we have to use steel shot or one of the other Non Lead shots to harvest the doves
BTW Full Body Goose decoys are a Great Morning Dove decoy :lol:
I was wondering if Zink could be used instead of a lead alloy with the drip and roll down the ramp into a cooling tank ?
As I have collected a fair amount of Zink WW's and a number of Zink anodes form junk boats
I know Zink needs a higher temp to melt , as I cast Zink decoy weights instead of using lead
Thanks
John
So if not feel free to move it
OK I make some of my own shot
Drip and roll into a cooling tank method
But I got to thinking last night
We do a lot of Morning Dove hunting as we wait for the Canada geese to decide to fly
As we are going to be also hunting geese , we have to use steel shot or one of the other Non Lead shots to harvest the doves
BTW Full Body Goose decoys are a Great Morning Dove decoy :lol:
I was wondering if Zink could be used instead of a lead alloy with the drip and roll down the ramp into a cooling tank ?
As I have collected a fair amount of Zink WW's and a number of Zink anodes form junk boats
I know Zink needs a higher temp to melt , as I cast Zink decoy weights instead of using lead
Thanks
John