View Full Version : Third Casting
aaholland
10-15-2016, 06:29 PM
Third casting session went better. Probably about 30% rejects. Considering the MiHec was brand new I dont think that is bad.
300 blackout is a NOE .311 230 grain Flat nose. A fellow forum member yondering removed the lube groves. It now drops around 244 grains.
9mm is a MiHec .359-125grain (9mm) HP Flat base.
http://i66.tinypic.com/1jrqq8.jpg
gwpercle
10-15-2016, 07:16 PM
Doing good...third time's the charm.
Actually moulds , especially aluminum and brass , need to be broken in, the cavities will develop a coating only achieved by casting. Mine start acting right after three heat cycling sessions ( no casting just heating and let slowly cool ) and then after the third casting session, they are good to go.
Gary
aaholland
10-16-2016, 04:17 PM
Powder coated today.
http://i67.tinypic.com/bi9uhh.jpg
bigolsmokebomb
10-17-2016, 10:06 PM
those look good. your PC job looks a lot better than mine but it may be the powder you're using too. all ive got is the good ol HF red
aaholland
10-18-2016, 05:38 AM
Its smokes powder. A guy from this form. I actually do two thin coats. With the 300 blackout i actually rub off the powder off the top of the bullet so the driving area is only thickly covered.
Boolseye
10-19-2016, 08:45 PM
Pretty molds.