11-08-2014, 11:16 PM
hey-Hey!!!,
I just got a 22596 and ran some low-tin/mostly lead boolits for my air rifle. Boolits *NEARLY* jumped out of the mold. I switched to a significantly harder alloy( the ingots ring, and I added a pinch of Tin for good measure ), and now the boolits don't want to leave. I mean, 40 year old virgin, on large allowance from parents, not-want-to-leave...took a fair bit of banging on the handles with my poplar board to get them to leave the cavity. In both cases, good fill, and in the harder alloy, no frosting or bluing...but they won't leave.
Any help greatly appreciated.
cheers,
Douglas
I just got a 22596 and ran some low-tin/mostly lead boolits for my air rifle. Boolits *NEARLY* jumped out of the mold. I switched to a significantly harder alloy( the ingots ring, and I added a pinch of Tin for good measure ), and now the boolits don't want to leave. I mean, 40 year old virgin, on large allowance from parents, not-want-to-leave...took a fair bit of banging on the handles with my poplar board to get them to leave the cavity. In both cases, good fill, and in the harder alloy, no frosting or bluing...but they won't leave.
Any help greatly appreciated.
cheers,
Douglas