.222 Rem TC Contender 8" Octagon Factory Barrel
Bore: .2245~ (approximate)
Groove: .2250 (3 measurements all came up the same, three different points on the cast)
Throat: .257
Bore slugged at the same time and came out the same as the chamber cast. Groove, which I can accurately measure came out to .2250 on the nose. Bore is an estimate as I don't have any way to measure that small a spot except with Calipers.
Could someone advise what I should have my Lee push through sized to? .225 or .226?
My Lee Bator mold drops Pure at .225 average of 25 boolits.
I plan on using Pistol powders and dacron for a 100% fill as I am wasting a lot of IMR4227 from the 8" barrel, and the next fastest powders I have are Alliant Steel and Longshot. I did find the thread with load data for Longshot in the .222
I intend to use this both for small critter and IHMSA Half Size as well as just all around plinking.
Any analysis of the cast would be appreciated!
.222 Rem TC Contender 8" Octagon Factory Barrel
Bore: .2245~ (approximate)
Groove: .2250 (3 measurements all came up the same, three different points on the cast)
Throat: .257
Bore slugged at the same time and came out the same as the chamber cast. Groove, which I can accurately measure came out to .2250 on the nose. Bore is an estimate as I don't have any way to measure that small a spot except with Calipers.
Could someone advise what I should have my Lee push through sized to? .225 or .226?
My Lee Bator mold drops Pure at .225 average of 25 boolits.
I plan on using Pistol powders and dacron for a 100% fill as I am wasting a lot of IMR4227 from the 8" barrel, and the next fastest powders I have are Alliant Steel and Longshot. I did find the thread with load data for Longshot in the .222
I intend to use this both for small critter and IHMSA Half Size as well as just all around plinking.
Any analysis of the cast would be appreciated!