GP100man
09-06-2007, 07:26 PM
some time back i asked about battery cable ends & if they were pure or alloyed .
well today is week 3 on curing time on the 2 batches cast .
both batches are the lee 158gr.rf boolit, one batch is stick on WW the other is the cable ends.
when smelted i pour a 3# ingot in a angle iron mould i cut a piece of 95/5 lead free solder the length of the ingots to help fillout which was needed.
the boolits from the cable ends are averaging 10.2 bhn & the stick on 8.7 bhn
i tested 25 boolits per batch.
just a follow up on a question i had to answer my self & one more roundtoit done!!!!!
GP100man:-D
:cbpour:
well today is week 3 on curing time on the 2 batches cast .
both batches are the lee 158gr.rf boolit, one batch is stick on WW the other is the cable ends.
when smelted i pour a 3# ingot in a angle iron mould i cut a piece of 95/5 lead free solder the length of the ingots to help fillout which was needed.
the boolits from the cable ends are averaging 10.2 bhn & the stick on 8.7 bhn
i tested 25 boolits per batch.
just a follow up on a question i had to answer my self & one more roundtoit done!!!!!
GP100man:-D
:cbpour: