GBCAPT
05-14-2012, 09:58 PM
I have only recently begun casting lee CTL-312-160 s for my CZ527 7.62X39.
Currently water quenching, adding aluminum gas checks, and tumble lubing with ALOX before loading as-cast over Red Dot & 800X for fun shooting in the local sand pit.
However. looking ahead to the next hunting season, I am considering going to full power loads after heat treating the same bullets.
I also would like to modify the boolits to a more flat pointed configuration if possible.
Anyone have any recommendation about an economical way to trim the meplat large enough to work well as a hunting bullet?
Currently water quenching, adding aluminum gas checks, and tumble lubing with ALOX before loading as-cast over Red Dot & 800X for fun shooting in the local sand pit.
However. looking ahead to the next hunting season, I am considering going to full power loads after heat treating the same bullets.
I also would like to modify the boolits to a more flat pointed configuration if possible.
Anyone have any recommendation about an economical way to trim the meplat large enough to work well as a hunting bullet?