I'm one of the new guys here. Been reading alot and trying to get my ducks in a row. Basically need lead for BP and SP loads. Bought some lead, got some lead dust given to me and today made a deal for some COWW no SOWW. The owner of the tire store said he'd give me three 5 gallon buckets full for $20.00/bucket.
Now if I am correct in my information, there will be between 50 and 70 punds of casting material that I can recover from each bucket. Makes the WW material about $0.30 -$0.40 per pound. Guess I can live with that.
Now if I am correct in my information, there will be between 50 and 70 punds of casting material that I can recover from each bucket. Makes the WW material about $0.30 -$0.40 per pound. Guess I can live with that.