When preheating bullets, what temperature do you "shoot" for ?
I've read 150 to 300 so i really don't know.
When preheating bullets, what temperature do you "shoot" for ?
I've read 150 to 300 so i really don't know.
Lake Havasu City... Born and raised
I think most coatings melt at 200 degrees; so 150 is what I do.
Sent from my iPhone using Tapatalk Pro
I preheat to 400F, that is the baking temp.
EVERY GOOD SHOOTER NEEDS TO BE A HANDLOADER.
NRA Cert. Inst. Met. Reloading & Basic Pistol
Preheat= so the powder adheres a bit better to the bullets compared to coating room temperature bullets.
Preheat to 400 degrees?
I would like to see bullets preheated to 400 degrees then coated with powder, then baked at 400 degrees.
Please show us those bullets.
http://
I set those in the oven to warm them up it was set at 400 for baking pulled them out and sprayed them then back in the oven to cook now you have see those bullets
Reloading to save money I am sure the saving is going to start soon
Understand how u heated.
Definitely not preheated to 400
Sent from my iPhone using Tapatalk Pro
My concern is a new coater tries heating to 400 then coating or attempting.
Sent from my iPhone using Tapatalk Pro
Preheating lead bullets before tumbling them in powder
Lake Havasu City... Born and raised
I shoot for 120 - 150 °F when I want to do my ASBB HF Red with high humidity.
Above around 150 °F lots of nonmetallic stuff starts being affected. This is also about the limit for an average person to hold their fingers on a hot surface.
Anything where all of the boolits actually get "very warm" (say 120 °F or above) seems to the good enough to counteract the humidity and allow a goood coating with a normal amount of swirling / shaking.
And FYI, it worked great last Sunday when I did a batch of 500 Lee 120 TC 9mm boolits.
Last edited by P Flados; 11-07-2017 at 11:10 PM.
I found that while heating the oven I can use the heat during the preheat time to my advantage. When the oven is about 10 degrees above room temp I put the bullets in for 20-30 seconds and pull them out. I bare handed touch them and if they are not too hot to touch I dump them into the powder coat. Once the oven is up to temp (400 degrees) then 10-12 seconds does the trick. For warming the Bullets go into the pan without anything separating them from the metal pan. For baking I use a silicone sheet. One layer of bullets with a little space between if possible. Oven heat controlled by a PID.
a m e r i c a n p r a v d a
Be a Patriot . . . expose their lies!
“In a time of deceit, telling the truth is a revolutionary act.” G. Orwell
I never preheat. Here in the desert SW, we don't get cold enough or wet enough to worry about it.
I would never to above 130 or so. Any higher the powder might clump in globs. If ESPC'ing you could heat a little more because the gun puts on an even coat.
But I get perrrrrrrfect coats without any heating at all. Do whatever floats your boat.....just do not get them too hot.
BP | Bronze Point | IMR | Improved Military Rifle | PTD | Pointed |
BR | Bench Rest | M | Magnum | RN | Round Nose |
BT | Boat Tail | PL | Power-Lokt | SP | Soft Point |
C | Compressed Charge | PR | Primer | SPCL | Soft Point "Core-Lokt" |
HP | Hollow Point | PSPCL | Pointed Soft Point "Core Lokt" | C.O.L. | Cartridge Overall Length |
PSP | Pointed Soft Point | Spz | Spitzer Point | SBT | Spitzer Boat Tail |
LRN | Lead Round Nose | LWC | Lead Wad Cutter | LSWC | Lead Semi Wad Cutter |
GC | Gas Check |