That is interesting.
I wonder if it was letters for a newspaper headline.
The most interesting thing sort of like that I've found in a scrap yard was about a foot thick stack of Tin
sheets for printing something in Brail.
In school: We learn lessons, and are given tests.
In life: We are given tests, and learn lessons.
OK People. Enough of this idle chit-chat.
This ain't your Grandma's sewing circle.
EVERYONE!
Back to your oars. The Captain wants to waterski.
Just out of curiosity I searched on "United American Metals"
They have a logo similar to the one on yours, a side facing Indian in a war bonnet.
Looks like they mostly made babbitt, were involved in government contracts in WW2.
You may have a collector's item there....nice find!
.
OK, I see it now.
The HYTIN might be to show what it is, and the block is shipped like that.
In school: We learn lessons, and are given tests.
In life: We are given tests, and learn lessons.
OK People. Enough of this idle chit-chat.
This ain't your Grandma's sewing circle.
EVERYONE!
Back to your oars. The Captain wants to waterski.
check wikipedia for monotype
HYTIN, High Tin? /Ingots for making solder bars for old time car body repair and such? I say old time and yet I have done auto body work with lead and solder. That's depressing!
That is not printing type. Monotype, Linotype for printing is/are reversed stand about 1" tall.
i believe they are for the wiped joints on lead pipes, basically a tin rich lead for joining the lead pipe to things like a lead trap.
if you are ever being chased by a taxidermist, don't play dead
Found a link: Stereotype???
https://books.google.com/books?id=bm...tin%22&f=false
Can't get more definitive than that!
Not likely. If it's babbitt, it would have become a machine bearing. Even during WW2, most engine bearings, even in aircraft engines, were still poured and scraped babbitt, so pieces like this would have been in every engine rebuilder's shop.
The steel-backed inserts we all know today were still experimental at the start of that war.
Babbitt almost always has some copper in it for strength.
The wiping solder hypothesis is still in the running, but my sources say it was about 60% lead, 40% tin. Not even the 50-50 we commonly use for sweated joints.
Cognitive Dissident
that copper is nice.. easy way to harden up a bullet mix without sacrificing as much weight.
A few years ago an acquaintance gave me some GC bullets he had cast in an Eagan mould from a babbitt alloy. Very hard, and they shot the lights out from a K31 I was enamored of at the time, loaded to 2200 fps!
Cognitive Dissident
For in much wisdom is much grief: and he that increaseth knowledge increaseth sorrow. Ecclesiastes 1:18
He that troubleth his own house shall inherit the wind: and the fool become servant to the wise of heart. Proverbs 11:29
...Verily I say unto you, Inasmuch as ye have done it unto one of the least of my brethren, ye have done it unto me. Matthew 25:40
Carpe SCOTCH!
Let us know what the composition turns out to be.
Cognitive Dissident
BP | Bronze Point | IMR | Improved Military Rifle | PTD | Pointed |
BR | Bench Rest | M | Magnum | RN | Round Nose |
BT | Boat Tail | PL | Power-Lokt | SP | Soft Point |
C | Compressed Charge | PR | Primer | SPCL | Soft Point "Core-Lokt" |
HP | Hollow Point | PSPCL | Pointed Soft Point "Core Lokt" | C.O.L. | Cartridge Overall Length |
PSP | Pointed Soft Point | Spz | Spitzer Point | SBT | Spitzer Boat Tail |
LRN | Lead Round Nose | LWC | Lead Wad Cutter | LSWC | Lead Semi Wad Cutter |
GC | Gas Check |