I started out at 710F and got some shrinkage mid bullet. Lowered the temp incrementally to 660 with the same results. Came back up to 775 which eliminates the shrink but now have whiskers, base is frosted and slow process time as the sprue must cool longer. Any words of experience in casting this alloy? Thanks