Hi
I have been casting boolits for about a year now and I am using HiTek to coat it.
I have recently changed over from a stock 2 Tanfo to CZ shadow 2
The problem I have now it's the S2 barrel is leading up.
This is what I have done thus far.
Lead hardness is 14/15
Changed lead to new lead
Changed coating to different combination of coating and passed acetone and Smash test..
Bought Cast Boolits from a manufacturer who sells these and his process is perfect.
Everyone one of them is leading and quickly too.
Heres a Pic after 50 rounds.
Any input will be appreciated
Sent from my VOG-L09 using Tapatalk