I am working on a batch of 68g, 22 Rim fire bullets. I'm too the point I can make the bullets turn out looking to my satisfaction. Now I'd like to try bonding the cores to jackets. I am not going to use any flux to begin with, I want to figure out a routine first. The problem is standing the Jacket/Core combo up while heating. The only thing I've found so far that fits the bill is a Tin bottom from .177 cal. pellets I found that fits 102 bullets at once, and I've only got one. I'm looking for a little higher production rate. My question to you is how do you stand them up while heating ?
My kiln capacity is advertised as 8x8x6 inch, but my ideal of a tray would only be 7x7x.5 inch the way I see it. But then on the other hand, if I didn't produce enough bullets in a batch, I'd have to have some way to keep them stood up somehow. Got any Idea's ???