Hey guys,
I have the Lee 00 buckshot mold that can drop eighteen pellets per pour. I have tried casting with "pure" lead (from melted birdshot), WW lead, and Lyman #2 alloy.
I have been unsuccessful in getting good fillout while using "pure" lead or WW lead, no matter how hot I get the melt or mold.
The only way I can get good fillout (~85-90% of all cavities filled completely per pour) is by using Lyman #2.
I'd prefer to save my Lyman #2 alloy for other casts though.
What alloy are you successful with when using the Lee 00 buck mold, and at what temp?
Thanks!