Hello,
Smelted about 17 pounds of WW tonight. Hand sorted with a cutter and removed FE and ZN. Used a turkey fryer and melted clip on Pb down. Set the stick on aside. Temperature read about 550 F once all melted.. Fluxed twice with cedar shavings. Attached are some photos. Any reason for concern based on the pictures?
How long should it take to flux (adding shavings to skimming out)?
Does any one add all ww and skim out the FE and ZN, assuming temp is kept below 700 F?
Thanks,