    metal prepping was done in my blasting cabinet using 120 grit aluminum oxide as per recomended at Lauers website. on the muzzel end i used play dough to protect the rifling. whatever you use to blast with make sure you use a good breathing respirator to keep it out of your lungs. next up is my Ruger single six after i reline the barrel.HTH. one more thing what grit is that aluminum oxide you got from harbor freight? also the 10/22 reciever is aluminum so don't worry about the 120 grit oxide doing damage to it.
    Rick
    Last edited by Rick459; 04-15-2010 at 12:10 AM.

  2. #42
    Banned

    PatMarlin's Avatar
    Join Date
    Aug 2005
    Posts
    6,341
    How'd I miss this thread Taylor?

    Lookin' like a cool project.

  3. #43
    Boolit Buddy
    Join Date
    Dec 2008
    Location
    San Diego
    Posts
    266
    Thanks!

    As far as the grit of my abrasive, it's pretty fine stuff I'll see if it's got a label.

    Hoping to hook up tomorrow (Thurs) with my buddy, we have a coinciding 2-hr window. If something screws that up, I'm about at the point of taking sandpaper to it just to get the project moving again.

  4. #44
    Boolit Buddy Wrbjr's Avatar
    Join Date
    Feb 2011
    Location
    Winter Haven, FL
    Posts
    246
    hmmm I guess by now those supplies from Dura Coat are pretty stale... ha ha....

  5. #45
    Boolit Buddy
    Join Date
    Dec 2008
    Location
    San Diego
    Posts
    266
    LOL maybe. I checked them about a month ago and they actually might still be viable. Obviously this project has gone nowhere, I really ought to do something with it.

  6. #46
    Boolit Buddy Rick459's Avatar
    Join Date
    Jan 2006
    Posts
    485
    Tippet,
    if ypu were a little closer you could bring it to my place and i would bead blast it for you for free..just to help you along to help you complete your project..
    Rick

  7. #47
    Boolit Buddy
    Join Date
    Dec 2008
    Location
    San Diego
    Posts
    266
    I appreciate it Rick, that is where I'm stuck. I think i can do a good enough job of it just with sandpaper. Just need to to take the time

  8. #48
    Boolit Buddy Rick459's Avatar
    Join Date
    Jan 2006
    Posts
    485
    i wonder if we have any forum members that are in the San Diego area with a blasting cabinet that could help you out.
    Rick

  9. #49
    Boolit Buddy
    Join Date
    Dec 2008
    Location
    San Diego
    Posts
    266
    Actually at the moment I have other things holding me up. Once I have some free time, I'm pretty sure I can do what I need to do using sandpaper

Page 3 of 3 FirstFirst 123

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check