    Casting alloy for 32 Mag hollow points

    Starting with clip on WW what should I add in order to get reliable expansion from a hollow point in a 32 H&R mag leaving a 6.5" barrel at 1,000-1,100 fps? Thank you.

  2. #2
    Boolit Buddy
    Join Date
    Dec 2009
    Location
    Ball Ground, GA
    Posts
    416
    In my test with 38 special and 357, the antimony content in coww will cause the nose to break off. If I blended the ww down with pure lead to at least 1% antimony and had the tin at 4/5% I had ok results from 850 to a 1000 fps.
    I switched to 20:1 and deep hp's did good starting at 850 up to 950. After 950 I had to use the cup points (shallow hp). Anything over 1000 or so 16:1 and cup points did better.
    If I really wanted the classic mushroom without losing weight on impact I would use 16:1 and cup points right around 950 to 1050. I had no leading with any of these. Hope my results are of some use to you.
    Tony

  3. #3
    Boolit Buddy

    Join Date
    Nov 2011
    Location
    Wisconsin
    Posts
    172
    Thank you Tony. Great info. Looking forward to trying it very soon.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check