    I have acquired a good supply if ingots. Smelted by unknown source.

    There is a large quantity of bars Some are marked LY#2, COWW, SOWW/Lead, BISMUTH & LY#3. Just a few Bismuth and most are SOWW/LEAD.

    I have Never herd if #3 as a "hardness". Do anyone know what this might be?

    Any help appreciated. There is only a small qualtity of these maybe 25 bars but wont waste it!

    Thanks guys

    CW
    NRA Life member • REMEMBER, FREEDOM IS NOT FREE its being paid for in BLOOD.
    Come visit my RUMBLE & uTube page's !!

    https://www.RUMBLE.com/user/Cwlongshot
    https://youtube.com/channel/UCBOIIvlk30qD5a7xVLfmyfw

  2. #2
    Boolit Master dbosman's Avatar
    Join Date
    Feb 2013
    Location
    East Lansing, MI, USA
    Posts
    1,995
    Lyman #2 is harder than #3, but of course I can't find the ratio, online.

    From this forum, from yovinny 11-28-2011, 10:08 AM
    Ideal #2- the 90/5/5 alloy commonly called Lyman #2 today.
    Ideal #4- 1 in 20 tin/lead alloy.
    Ideal #6- 1 in 40 tin/lead alloy.

  3. #3
    Boolit Grand Master


    Larry Gibson's Avatar
    Join Date
    Jul 2005
    Location
    Lake Havasu City, Arizona
    Posts
    21,326
    #3 alloy was 1 in 10 tin/lead alloy. #1 was 80/7/3/10 lead/antimony/tin/copper [the % of Sb and Sn varies with source].
    Larry Gibson

    “Deficient observation is merely a form of ignorance and responsible for the many morbid notions and foolish ideas prevailing.”
    ― Nikola Tesla

  4. #4
    Boolit Master
    Join Date
    Feb 2008
    Location
    Finger Lakes Region of NY
    Posts
    1,254
    Quote Originally Posted by Larry Gibson View Post
    #3 alloy was 1 in 10 tin/lead alloy. #1 was 80/7/3/10 lead/antimony/tin/copper [the % of Sb and Sn varies with source].
    Thanks for that info, Larry. Dang, with that much copper, that #1 had to be one hard alloy.

    Don
    NRA Certified Metallic Cartridge Reloading Instructor
    NRA Life Member

  5. #5
    Boolit Grand Master


    Larry Gibson's Avatar
    Join Date
    Jul 2005
    Location
    Lake Havasu City, Arizona
    Posts
    21,326
    Yes, #1 is a very hard alloy. It was considered the "standard" alloy for numerous Ideal bullet moulds for use in 30 - 8mm rifles, mostly military, in the late 1800s and early 1900s. Also, #1 alloy gave considerable shrinkage which is why many of those earlier Ideal moulds will cast .002 -.004" over nominal diameter with #2 alloy or linotype.
    Larry Gibson

    “Deficient observation is merely a form of ignorance and responsible for the many morbid notions and foolish ideas prevailing.”
    ― Nikola Tesla

  6. #6
    Boolit Master


    cwlongshot's Avatar
    Join Date
    Jul 2012
    Location
    Central Connecticut
    Posts
    3,735
    Thank you everyone!!

    The #3 rings more then thuds but no where near the ring of the #2!

    CW
    NRA Life member • REMEMBER, FREEDOM IS NOT FREE its being paid for in BLOOD.
    Come visit my RUMBLE & uTube page's !!

    https://www.RUMBLE.com/user/Cwlongshot
    https://youtube.com/channel/UCBOIIvlk30qD5a7xVLfmyfw

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check