    This is the alloy I was using for bullets. According to my notes it should be about 95% lead, 2.5%tin, 2.5% antimony. 11-12 hardness. Again, as with all this stuff it is an educated guess. There is 55 lbs, will be packed into 4 SFRB which will then be placed in a MFRB and braced with plywood top and bottom. That is about the best I can pack it. $80 shipped

  2. #2
    Boolit Buddy
    Join Date
    Feb 2016
    Location
    S.E. Michigan
    Posts
    414
    If you take paypal, I will take it.

  3. #3
    Banned
    Join Date
    Apr 2013
    Location
    Northern California
    Posts
    1,029
    I'll take it.

    pm sent.

    Steve in N CA

  4. #4
    Boolit Buddy
    Join Date
    Oct 2013
    Posts
    452
    Looks like Dimner got it posted first. SPF to Dimner

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Abbreviations used in Reloading

BP Bronze Point IMR Improved Military Rifle PTD Pointed
BR Bench Rest M Magnum RN Round Nose
BT Boat Tail PL Power-Lokt SP Soft Point
C Compressed Charge PR Primer SPCL Soft Point "Core-Lokt"
HP Hollow Point PSPCL Pointed Soft Point "Core Lokt" C.O.L. Cartridge Overall Length
PSP Pointed Soft Point Spz Spitzer Point SBT Spitzer Boat Tail
LRN Lead Round Nose LWC Lead Wad Cutter LSWC Lead Semi Wad Cutter
GC Gas Check